Aluminized Steel Sheet – SA1C, SA1D & SA1E

Type I aluminized steel sheet with an aluminum-silicon coating for formed components, heat reflectors and industrial applications.

  • Grade options: SA1C, SA1A, SA1D and SA1E; structural references SAC31, SAC35, SAC41 and SAC45.
  • Coating: aluminum-silicon, with approximately 8–10% silicon in the bath.
  • Post-treatment: chromated, oiled, chromated and oiled, or untreated.

Send your grade, dimensions, coating requirements, quantity and application for a quotation. Heat-test results and mechanical conditions are detailed below.

Description

Type I Aluminized Steel Sheet – SA1C, SA1D & SA1E

Fullgreat supplies hot-dip aluminized steel sheet for formed components requiring heat reflectivity, heat resistance and protection of the steel surface. This page focuses on Type I aluminum-silicon coated steel, with commercial and drawing grades including SA1C, SA1D and SA1E, plus the structural grades listed below.

The steel substrate provides the mechanical properties, while the aluminum-silicon coating contributes surface protection and reflectivity. The coating bath contains approximately 8–10% silicon, with aluminum as the principal constituent. This material is distinct from solid aluminum sheet, aluminum-zinc-coated steel and zinc-aluminum-magnesium coated steel.

Key Features

Heat Resistance & Surface Appearance

Aluminized steel is used where a coated steel surface must resist heat-related discoloration. The comparison below records surface appearance after the stated thermal cycles. Select the material for the component’s actual metal temperature, exposure duration and environment.

Heat Resistance Test Results

Visual assessment after two test cycles; each cycle comprised heating for 1.5 hours, holding for 5 hours and cooling for 17 hours. The temperature columns show the test conditions, rather than continuous-service ratings.

Material300°C350°C400°C450°C500°C550°C600°C
Aluminized Steel○○○○○○~△×
Aluminum-zinc-coated steel○○△△~××××
Galvanized steel (GI)△△~××××××

○: no visible change; △: reduced luster; ×: blackish discoloration. These symbols describe appearance, rather than retained strength, corrosion life or complete component performance.

Heat Reflectivity

The heat-exposure comparison below lists 80% reflectivity for aluminized steel after 24 hours at both 100°C and 450°C. This supports consideration for reflector components in ovens, toasters and heating equipment. Reflector performance also depends on wavelength, surface condition and component geometry.

ClassificationAluminized SteelGalvanized steel (GI)
100°C × 24 hr80%80%
450°C × 24 hr80%15%

Specifications

Coating Types

Type I uses an aluminum-silicon coating and is the focus of this product. Type II uses an aluminum coating and is included here to distinguish the two material types.

ClassificationType I AluminizedType II Aluminized
Molten bath componentsAluminum with 8–10% siliconAl
ApplicationHeat-related applicationsWeather-exposure applications, including construction

Mechanical Properties

The reference tables below retain the stated thickness conditions and property limits. Strength is expressed in kgf/mm² (1 kgf/mm² ≈ 9.81 MPa). Specify the required grade, standard edition, thickness and mechanical properties for the order.

Grade referenceTensile min (kgf/mm²)Yield min (kgf/mm²), t ≤ 0.5 mmYield min (kgf/mm²), t > 0.5 mmElongation min (%), t ≤ 0.5 mmElongation min (%), 0.5 < t ≤ 1.2 mmElongation min (%), t > 1.2 mm
SAC31 / SQ-A312121202020
SAC35 / SQ-B352525202020
SAC41 / SQ-C413030181818
SAC45 / SQ-D453737181818
GradeHardness HR30T maxYield (kgf/mm²), t ≤ 0.5 mmYield (kgf/mm²), 0.5 < t ≤ 2.3 mmTensile (kgf/mm²)Elongation (%), t ≤ 0.5 mmElongation (%), 0.5 < t ≤ 1.2 mmElongation (%), t > 1.2 mm
SA1C6526–3626–3636–4234–4034–4034–40
SA1D50≤24≤23≥28≥36≥38≥40
SA1E48≤21≤20≥28≥38≥40≥42

Grade & Specification References

The lists below help identify purchasing designations. They group reference names without authorizing direct substitution between standards. State the complete grade, coating and standard edition when ordering.

Specification systemDesignationsOrdering consideration
JIS G3314SA1C; SA1A; SA1D; SA1E; SAC31; SAC35; SAC41; SAC45Select the complete grade and required coating designation.
ASTM designation referencesCQ; ADQ; DQ; DQSK; EDDQ; SQ-A/B/C/D; CS Type A/B/C; FS; DDS; EDD; Grades 230, 255, 275, 340 Class 1/2/3 and 550Terminology depends on the specified edition; include the complete ASTM A463/A463M requirement.
European designation referencesDX51D, DX52D, DX53D, DX54D, DX55D; S250GD, S280GD, S320GD, S350GDInclude the governing standard, coating designation and required properties; grade names alone do not define the complete coated product.

Post-treatment Options

TreatmentChromatedOiledChromated & OiledNo Treatment
Availability○○○○

Chromate-treatment reference: average 11.5 mg/m² per side, with a range of 6.8–18.9 mg/m² per side. Oil application references, total for both sides: light 500–800 mg/m², normal 1,000–1,400 mg/m² and heavy 1,400–2,000 mg/m². These figures describe post-treatment, separately from the aluminum-silicon coating mass.

Choose the post-treatment for storage, handling and subsequent forming, joining or painting requirements. Include any restrictions on surface treatment in the purchasing specification.

Applications

  • Automotive components: mufflers, exhaust pipes, fuel tanks
  • Home electrical appliances: electric stoves, gas ranges, bread machines, toasters, frying pans, dryers, rice cookers
  • Heating equipment: heat exchangers, stovepipes, pre-heaters, dryers, ducts
  • Construction: walls and roofs of chemical factories, fireproof walls
  • Other: steam covers, chemical equipment

Applications describe material-selection opportunities. For exhaust parts, heating components or fire-wall assemblies, the finished design and operating conditions determine the required material specification and component acceptance requirements.

Aluminized Steel FAQ

Which grade should I select for forming?

SA1C covers commercial-quality requirements; SA1A, SA1D and SA1E are drawing-grade references. The structural range includes SAC31, SAC35, SAC41 and SAC45. Select the grade for the most demanding bend or drawn feature and the strength needed in the finished part.

How is this different from aluminum sheet or aluminum-zinc-coated steel?

This product has a steel substrate with an aluminum-silicon coating. Solid aluminum sheet has an aluminum base, while aluminum-zinc-coated steel uses a different coating composition. Choose the material specification for the required mechanical, forming and exposure conditions.

Does the 450°C test establish the operating temperature of my part?

The tables describe surface appearance after thermal cycles and reflectivity after stated heat exposure. Actual component selection also considers metal temperature, exposure time, atmosphere, mechanical loading and the condition of formed or joined areas.

What should I include in a quotation enquiry?

Send the grade and standard, required thickness and width, supply form, quantity, coating designation or mass requirement, and post-treatment. Include the forming process, service conditions, delivery destination and any inspection requirements relevant to the component.